Different JIGS

Different JIGS

DIFFERENT JIGS FOR

 

i.  FATIGUE LIFE OF COMPACTED HMA SUBJECTED TO REPEATED FLEXURE BENDING

  • Fatigue life and energy for 380 mm long x 50 mm thick x 63 mm wide beam specimens of laboratory or field compacted HMA subjected to repeated flexure bending until failure can be obtained.

ii. INDIRECT TENSILE STRENGTH
   (EN 12697-26:2004 & ASTM D6931-2007)

 

  • Can Determine the Dynamic and Static creep characteristics of bituminous mixtures by means of an uniaxial cyclic compression test and creep characteristics of bituminous mixtures by means of the triaxial cyclic compression test.